• Time: 60 Seconds
• Temp: 356 F (182 C)
• Heavy Pressure.
Please ensure both protective films are completely removed from the front and back of the material prior to printing to prevent the film from melting under high heat. Immediately following the print cycle, place a heavy, flat object evenly over the material to ensure flatness and prevent warping.